I have a 3d printer, and right now I am only using PLA which has a relatively low melting temperature (hot car in the sun or dishwasher would be enough to warp it).
I am interested in printing some gear parts like trekking pole baskets or contoured maps or scope covers, is PLA going to warp from just being in the sun on a hot summer day?
Post
+1
−0
The glass transition temperature of PLA is around 60 C/140 F. It's unlikely to warp from direct sunlight alone, but PLA has two other characteristics that make it unsuitable for printing gear:
- PLA is brittle. Where something printed from PETG or ABS would flex and absorb a blow, PLA will crack.
- PLA is highly susceptible to creep. A constant force on a piece of PLA will cause it to flow, permanently changing the shape of the part.